To contact us for more information on this product click here >>

  • Description

    PPG CORAFLON ADS (Air-Dry System) is a field-applied fluoropolymer that delivers factory applied performance in a two-component air-dry system.  Meeting FGIA/AAMA 2605 standards for chemical and weather resistance, Coraflon ADS is ideal for new construction and the restoration of existing architectural metal.

  • Chemistry

    Two-component fluoropolymer FEVE resin

  • Application

    Shop or field-applied brush, roller or spray application for coil and extrusion

  • Benefits

    • Brilliant, low-maintenance, enduring finish
    • Excellent resistance to chalking, fading, marring, abrasion and UV light
    • Available in rich palette of solid, brighter mica and metallic finishes
    • Optimized for restoration of weathered architectural metals
    • Meets FGIA/AAMA 2605 standards for weatherability and chemical- resistance
    • 10-85 gloss range
    • Ideal for new and existing construction
  • Suggested End Uses

    • Building panels
    • Window mullions
    • Amusement park rides
    • Stadiums
    • Metal roofing
    • Corporate signage

Product Characteristics

Color Wide range of colors
Gloss at 60º (ASTM D523) Standard gloss is 30 and 80

Technical Properties

Property Standard Results
Dry Film Thickness ASTM D1400 Primer: consult PPG technical service / Topcoat: 1.5-2.2 mil
Pencil Hardness ASTM D3363 HB - H
Flexibility, T-Bend ASTM D4145 3 T-bend; no cracking or pick-off
Adhesion ASTM D3359 No adhesion loss
Impact Resistance ASTM D2794 No cracking or pick-off
Abrasion, Falling Sand ASTM D968 50 liters min.
Detergent Resistance ASTM D2248 / ASTM D3359 No adhesion loss
Acid Resistance ASTM D1308 10% sulfuric acid (24 hours, FGIA/AAMA 2605) - No discoloration; 10% nitric acid spot (15 minutes) - <5∆E color change; 10% muriatic acid spot (15 minutes) - No discoloration
Salt Spray Resistance ASTM B117 1,000 hours (steel) / 4,000 hours (aluminum) - 1/8" max. avg. scribe creep; none or few #8 field blisters
Humidity Resistance ASTM D714, ASTM D2247 1,500 hours (steel) / 4,000 hours (aluminum) - 1/8" max. avg. scribe creep; none or few #8 field blisters
Exterior Exposure ASTM D2244, ASTM D4214 10 years @ 45º, South Florida / Erosion - Max. 5 fade, max. 8 chalk / <10% loss after exposure